Logo
  Europe/Middle East/Africa
line
  Americas
line
  Asia/Pacific
line

[Flow characteristics of the mold]

The flow behavior of Desmopan® and Texin™ is basically the same as that of other thermoplastics. The length of the flow path is dependent on the melt temperature, the wall thickness of the part to be filled, the injection speed and the rheological properties of the material.

The injection speed can be varied according to the machine and the technical circumstances.

The following figure shows the flow path of Desmopan® and Texin™ as a function of melt temperature.

click to recieve an enlarged image (Pop-Up Window)
Fig. 13: Length of flow path as a function of temperature

 

To achieve maximum mechanical properties and to reduce the shrinkage of the part to a minimum it is necessary to process the material with the „optimum melt
temperature“.

Product-specific Data about the flow behaviour against the wall thickness at optimum melt temperature according to the example given in the table below, are available for most of our grades upon request.